22. Errors with processing of dental alloys.

Inside: 8 sections · 1 table · 7 min

Essay 22 of 85 in the MU Plovdiv syllabus for Dental Materials (Dental Medicine, Year 1). The free AceMed note covers it in 8 sections, about 809 words (7 min of reading).

In this note

  1. Introduction
  2. Classification of processing errors and casting defects
  3. Distortion and dimensional misfit
  4. Surface roughness, irregularities and discolouration
  5. Porosity (the most important group)
  6. Incomplete casting and rounded margins
  7. Errors in melting, cooling, pickling and finishing
  8. Errors in heat treatment, joining and metal-ceramic processing

Introduction

A cast restoration passes through a chain of steps: pattern, spruing, investing, burnout, melting and casting, cooling and pickling, finishing, heat treatment or soldering, and porcelain firing. An error at any step gives a defective, ill-fitting or weak restoration. Most errors can be prevented by knowing their cause.

Classification of processing errors and casting defects

By stage: wax pattern, spruing, investing, burnout, melting and casting, after-casting treatment (cooling, pickling, finishing, heat treatment), joining, and porcelain veneering.

The classic grouping of casting defects:

  1. distortion and dimensional misfit
  2. surface roughness, irregularities and discolouration
  3. porosity
  4. incomplete casting

In addition there are foreign-body inclusions and hot tears (cracks).

Distortion and dimensional misfit

  • Wax pattern distortion comes from release of internal stresses with temperature change, from delay before investing, or from careless handling (removal, thin margins). Prevention: invest promptly and handle the pattern carefully.
  • Uncompensated shrinkage: the alloy shrinks on solidification and cooling, by about 1.4% for gold alloys and more (about 2%) for base-metal alloys. The setting, hygroscopic and thermal expansion of the investment must compensate for this.
  • Too little expansion (no ring liner, wrong W/P ratio, too low a burnout temperature) gives a small, tight casting. Excessive expansion gives an oversized, loose casting.
  • Non-uniform expansion of the mould, from restraint by the ring, distorts the casting.