Dental Materials · MU Plovdiv

46. Changes and defects of acrylic resins.

Inside: 7 sections · 1 table · 5 min

Essay 46 of 85 in the MU Plovdiv syllabus for Dental Materials (Dental Medicine, Year 1). The free AceMed note covers it in 7 sections, about 594 words (5 min of reading).

In this note

  1. Introduction
  2. Dimensional changes: polymerisation shrinkage, thermal shrinkage, water sorption
  3. Porosity
  4. Internal stresses and warpage
  5. Crazing
  6. Fracture
  7. Colour change and residual monomer

Introduction

During processing and in service, acrylic denture-base resin undergoes dimensional changes and can develop defects: porosity, internal stress and warpage, crazing, fracture, colour change and residual monomer. Each has a known cause and a known way of preventing it, and a good answer links every defect to its cause.

Dimensional changes: polymerisation shrinkage, thermal shrinkage, water sorption

  • Polymerisation shrinkage: MMA monomer shrinks about 21% by volume on polymerising. Because most of the dough is prepolymerised powder (powder:liquid about 3:1 by volume), the dough shrinks only about 6-7% by volume. Clinically the linear change is small and spread evenly over the base.
  • Thermal shrinkage: the resin cools from the processing temperature while held by the gypsum mould, and its high coefficient of thermal expansion matters here. This is the main cause of the classic poor adaptation at the posterior palatal border of the upper denture.
  • Water sorption: the denture slowly takes up water and expands slightly, which partly compensates for the shrinkage. Dentures are therefore stored in water. Repeated drying and wetting cause dimensional change and crazing.